Common Defects Of Silk-screen Printing-Part Two

Dec 16, 2021

Leave a message

Common Defects Of Silk-screen Printing-Part Two


1. Misalignment: Due to the inaccuracy of the silk-screen position, the silk-screen position is shifted.


2. Poor adhesion: The silk-screen coating has insufficient adhesion and can be pasted off with 3M-810 adhesive tape.


3. Pinholes: pinholes can be seen on the surface of the coating film.


4. Scratches and scratches: caused by poor protection after silk screen printing.


5. Variety, stains: non-silk-printed colors adhere to the silk-printed surface.


6. Color difference: There is a deviation in color compared with the standard color plate.